1. Assessment of the reuse of Covid-19 healthy personal protective materials in enhancing geotechnical properties of Najran's soil for road construction: Numerical and experimental study.
- Author
-
Abdullah, Gamil M.S. and El Aal, Ahmed Abd
- Subjects
- *
ROAD construction , *COVID-19 , *COVID-19 pandemic , *CONSTRUCTION materials , *SOIL classification - Abstract
The COVID-19 pandemic has not only caused a global health crisis, but it has also had significant environmental and human consequences. During the COVID-19 pandemic, this study focused on emerging challenges in managing healthy personal protective materials (HPPM) in Kingdom of Saudi Arabia, using silty sand (SM) soil as an example since it covers large areas in KSA and in the whole world. The main objective of this paper is to find a novel way to minimize pandemic-related waste by using HPPM as waste materials in road construction. For the first time, a series of experiments was conducted on a mixture of different percentages of shredded HPPM (0, 0.5, 1 and 2%) added to the silty sand (SM) soil for road applications, including soil classification according to the USCS, modified compaction, UCS, UPV, and CBR. In addition, a numerical simulation was performed using geotechnical-based software Plaxis 3D to study the performance of the soil-HPPM mix as a subbase layer in the paving structure under heavy traffic loading. The modified compaction test results show that there is an increase in the optimum moisture content with increasing the HPPM contents from 0.5% to 1% and 2%. However, a reduction in the maximum dry density is observed. The values of dry density and water content at 0%, 0.5%, 1% and 2% pf HPPM are 2.045, 1.98, 1.86 and 1.8 g/cm3 and 7.65% 8%, 8.5% and 9.5%, respectively. The soaked CBR values at 0, 0.5, 1 and 2% HPPM are 23, 30, 8, 2% with the maximum value attained with the addition of 0.5% HPPM. The results of UCS were with the same percentages of HPPM 430, 450, 430 and 415 kPa, respectively, with the maximum value attained with 0.5% HPPM addition as well. In contrast, the values of UVP at 0%, 0.5%, 1% and 2% are 978.5, 680.3, 489.4 and 323.6 m/s, respectively, confirming the trends obtained by modified compaction test results. The simulation results confirm this conclusion that the soil-HPPM mix show a superior performance when used as a subbase layer and reduced vertical displacement by a percentage of 11% compared to the normal subbase material. By eliminating HPPM especially facemasks from the landfill lifecycle, incorporating them into high quality construction material production has the potential to deliver significant environmental benefits. [Display omitted] 1 Influence of polypropylene (HPPM) fibres on the performance of sandy soil is clearly studied. 2 The optimum fibres content is obtained as 0.5% volume fraction. 3 Positive improvement is also noticed in unconfined compressive strength and compaction after adding HPPM fibres. 4 Fibres play a major role in crack bridging. [ABSTRACT FROM AUTHOR]
- Published
- 2021
- Full Text
- View/download PDF