1. High Strain Rate Response of Cross-Linked and Linear PVC Cores.
- Author
-
Tonnia Thomas, Hassan Mahfuz, Krishnan Kanny, and Shaik Jeelani
- Subjects
FOAM ,POLYVINYL chloride ,MATERIALS ,STRAINS & stresses (Mechanics) - Abstract
The compressive response of cross-linked and linear PVC foam core materials, namely, H130 and HD130 having identical densities were evaluated. Both cores were subjected to compressive loading at various strain rates ranging from quasi-static to 1560 s1. At quasi-static loading, the compressive strength of the H grade was approximately 30% higher than the HD grade. On the other hand, at HSR loading the HD grade was 20% higher. HSR tests were also conducted at various temperatures ranging from 25 to 12°C. It was observed that degradation of strength was more severe for the HD grade as temperatures increased. A recovery of the cores original volume was also noticed during high strain rate and elevated temperature tests. Accordingly, residual properties were determined. Results show that only the residual properties of the HD grade were affected by temperature. [ABSTRACT FROM AUTHOR]
- Published
- 2004
- Full Text
- View/download PDF