Desorption of LiAlH4 with Ti- and V-based additives

Authors :
Blanchard, D.
Brinks, H.W.
Hauback, B.C.
Norby, P.
Source :
Materials Science & Engineering: B. Apr2004, Vol. 108 Issue 1/2, p54. 6p.
Publication Year :
2004

Abstract

Thermal desorption spectroscopy and X-ray diffraction experiments show that ball-milling of LiAlD4 in presence of VCl3 or TiCl3·1/3(AlCl3) can reduce its thermal decomposition temperatures by 60 and 50 °C, respectively. However, some partial decomposition of LiAlD4 into Li3AlD6, Al and D2 occurs during the mechanical processing: 80% for TiCl3·1/3(AlCl3), 40% for VCl3. LiCl is formed during the ball-milling, this suggests the reduction of the additives by LiAlD4. The localisations of Ti or V atoms are not yet determined. [Copyright &y& Elsevier]

Details

Language :
English
ISSN :
09215107
Volume :
108
Issue :
1/2
Database :
Academic Search Index
Journal :
Materials Science & Engineering: B
Publication Type :
Academic Journal
Accession number :
12741254
Full Text :
https://doi.org/10.1016/j.mseb.2003.10.114