Back to Search Start Over

FIRE-PROOF UNSATURATED POLYESTERS ON THE BASIS OF ANHYDRIDE OF HEXABROMOBICYCLO-[2,2,1]-HEPT-5-ENE-2,3-DICARBOXYLIC ACID, GLYCERIN AND METHACRYLIC ACID.

Authors :
Gahramanly, Y. N.
Mustafayev, A. M.
Babanly, B. N.
Hajiyeva, R. Sh.
Ismailova, R. I.
Source :
Chemical Problems / Kimya Problemləri. Jan2018, Vol. 16 Issue 1, p51-57. 7p.
Publication Year :
2018

Abstract

The paper deals with production of α, ω-methacryl-(bis-glycerin)- endomethylenehexabromotetrahydrophthalate (BNP) on the basis of anhydride of 1,4,5,6,7,7- hexabromobicyclo-[2,2,1]-hept-5-ene-2,3-dicarboxylic acid, glycerin and methacrylic acid. Kinetics of polycondensation is researched at 170-1900C. It is ascertained that the acid number equal 30-50 mg of KOH per 1 g of unsaturated polyesters is obtained at 1700C within 6 hours, at 1800C within 3.5 hours and at 1900C within 3 hours.The hardening of BNP samples with the acid number from 20 up to 80 mg of KOH per 1g of resin showed that gelatinization rate of the styrene solutions in the presence of 3% methylethylketone hydroperoxide and of 8% cobalt naphthenate considerably increases with the reduction of the acid number. It is ascertained that gelatinization time at 200C decreases in 6-6.5 times with the transition from BNP with the acid number of 20 mg of KOH per 1g of resin to BNP with the acid number of 80 mg of KOH per 1g of resin. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
22218688
Volume :
16
Issue :
1
Database :
Academic Search Index
Journal :
Chemical Problems / Kimya Problemləri
Publication Type :
Academic Journal
Accession number :
128773658
Full Text :
https://doi.org/10.32737/2221-8688-2018-1-51-