Cite
Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy.
MLA
Huang, Liying, et al. “Effects of Grain Size and Texture on Stress Corrosion Cracking of Friction Stir Processed AZ80 Magnesium Alloy.” Engineering Failure Analysis, vol. 92, Oct. 2018, pp. 392–404. EBSCOhost, https://doi.org/10.1016/j.engfailanal.2018.06.012.
APA
Huang, L., Wang, K., Wang, W., Yuan, J., Qiao, K., Yang, T., Peng, P., & Li, T. (2018). Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy. Engineering Failure Analysis, 92, 392–404. https://doi.org/10.1016/j.engfailanal.2018.06.012
Chicago
Huang, Liying, Kuaishe Wang, Wen Wang, Jie Yuan, Ke Qiao, Tao Yang, Pai Peng, and Tianqi Li. 2018. “Effects of Grain Size and Texture on Stress Corrosion Cracking of Friction Stir Processed AZ80 Magnesium Alloy.” Engineering Failure Analysis 92 (October): 392–404. doi:10.1016/j.engfailanal.2018.06.012.