- In order to investigate the sintering mechanism between Ti and A1 in low temperature stage, the low temperature internal friction behaviors of Ti/A1 composite powder compact were studied systemically based on internal friction measurement technology. The experimental results show that the internal friction performance of the Ti/Al composite powder compact has obvious temperature effect. During the temperature measurement, the peak value of the irreversible internal friction near 270 °C decreases with the increase of frequency, and increases with the increase of A1 content. It is caused by stress release and is a stress type internal friction peak. During the cooling process, the peak of internal friction peak near 230 °C shifts to the high temperature, and has a certain relaxation characteristic. The internal friction peak originates from the slip o£ the A1 boundary formed by recrystallization during the heating process of of Ti/A1 composite powder compact. [ABSTRACT FROM AUTHOR]
Details
- Language :
- Chinese
- ISSN :
- 20951744
- Volume :
- 9
- Issue :
- 9
- Database :
- Academic Search Index
- Journal :
- Nonferrous Metals Engineering
- Publication Type :
- Academic Journal
- Accession number :
- 139558090
- Full Text :
- https://doi.org/10.3969/j.issn.2095-1744.2019.09.008