Maximum energy product of exchange-coupled Sm(FeCo)12/α-Fe nanocomposite particle.

Authors :
Uda, Ryusei
Koike, Kunihiro
Inaba, Nobuyuki
Kato, Hiroaki
Itakura, Masaru
Okubo, Susumu
Ohta, Hitoshi
Tsuchiura, Hiroki
Source :
AIP Advances. Feb2023, Vol. 13 Issue 2, p1-7. 7p.
Publication Year :
2023

Abstract

The effects of the coating surface orientation of the α-Fe soft magnetic layer on the Sm(Fe0.8Co0.2)12 hard magnetic phase and the volume fraction of α-Fe, VFe, on the maximum energy product, (BH)max of exchange-coupled Sm(Fe0.8Co0.2)12/α-Fe nanocomposite magnet particles were micromagnetics OOMMF package was systematically investigated. The (BH)max of the reference model, Sm(Fe0.8Co0.2)12 particles without Fe layer, was 630 kJ/m3. In contrast, in the nanocomposite magnet particle model with soft magnetic layers on both sides of the hard magnetic phase, (BH)max reached a maximum value of 657 kJ/m3 at VFe = 12% (Fe layer thickness, tFe = 2 nm). In the model with α-Fe coating on the top and bottom surfaces of the hard magnetic phase, (BH)max = 636 kJ/m3 at VFe = 4% (tFe = 2 nm). Furthermore, the coating of the soft magnetic phase on both sides of the hard phase particles reduces the magnitude of the demagnetizing field, Hd of the nanocomposite magnet particles, indicating that the side coating of the soft magnetic phase is effective in increasing (BH)max. These findings allow for a greater degree of freedom in the design of nanocomposite magnets by adjusting not only the VFe volume fraction of the hard/soft phases but also their arrangement. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
21583226
Volume :
13
Issue :
2
Database :
Academic Search Index
Journal :
AIP Advances
Publication Type :
Academic Journal
Accession number :
162171638
Full Text :
https://doi.org/10.1063/9.0000506