Hysteresis phenomena in Cd2P2S6 layered crystals.

Authors :
Ban, H.
Gal, D.
Motrja, S.
Molnar, A.
Source :
Low Temperature Physics. Jan2025, Vol. 51 Issue 1, p49-54. 6p.
Publication Year :
2025

Abstract

The results of the study of the temperature dependence of the dielectric permittivity of Cd2P2S6 crystals are presented. It is shown that in the temperature range 80–420 K there are three regions in which hysteresis phenomena are observed. At high temperatures (T > 320 K) there is an activation change of the dielectric losses associated with the increased conductivity of Cd2P2S6 crystals. The transition from heating to cooling leads to a decrease in losses, which is manifested as a hysteresis in the dielectric constant. A jump-like change in dielectric permittivity is found at 228 K in the cooling mode and 265 K in the heating mode, which is due to the first-order phase transition in these crystals. The third hysteresis region appears at low temperatures of 80–90 K. When the temperature is cycled in this interval, the classical hysteresis behavior is observed with a decrease in both amplitude and temperature range with each cycle. The cause of this behavior will be the subject of further investigation. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
1063777X
Volume :
51
Issue :
1
Database :
Academic Search Index
Journal :
Low Temperature Physics
Publication Type :
Academic Journal
Accession number :
182618149
Full Text :
https://doi.org/10.1063/10.0034644