Abstract: To prevent carbon/carbon composites from oxidation at 1773 K, an efficient oxidation protective glass coating has been prepared on the surface of SiC coated C/C composites by a simple and low-cost method. The microstructures and phase composition of the as-prepared coating were examined by SEM and XRD. Oxidation testing shows, after oxidation in air at 1773 K for 140 h and thermal cycling between 1773 K and room temperature for 8 times, the weight loss of the coated sample is only 0.98%. The oxidation of the coated C/C composites is attributed to the formation of bubble holes on the coating surface and microcracks in the coating. [Copyright &y& Elsevier]

Details

Language :
English
ISSN :
0167577X
Volume :
60
Issue :
3
Database :
Academic Search Index
Journal :
Materials Letters
Publication Type :
Academic Journal
Accession number :
19058400
Full Text :
https://doi.org/10.1016/j.matlet.2005.09.006