Loss of carbonate ester bonds along Fe ion tracks in thin CR-39 films

Authors :
Yamauchi, T.
Watanabe, S.
Seto, A.
Oda, K.
Yasuda, N.
Barillon, R.
Source :
Radiation Measurements. Aug2008, Vol. 43, pS106-S110. 0p.
Publication Year :
2008

Abstract

Abstract: In order to identify the chemical modification along nuclear tracks in CR-39 detectors, we have made a series of FT-IR measurements for thin CR-39 plastic films irradiated by Fe ions. The films were reduced in the thickness by long time chemical etchings down to from as-received CR-39 sheets of thick. It enabled us to obtain unsaturated IR spectra. The samples were exposed to 147MeV Fe ions at HIMAC in air. Amount of loss of carbonated ester bonds due to the exposure was assessed from the changes in the absorbance of and bonds with Fe fluence. The assessed G-value for destroying carbonate ester bonds was found to be about 10 (scission/100eV). [Copyright &y& Elsevier]

Details

Language :
English
ISSN :
13504487
Volume :
43
Database :
Academic Search Index
Journal :
Radiation Measurements
Publication Type :
Academic Journal
Accession number :
33776402
Full Text :
https://doi.org/10.1016/j.radmeas.2008.04.044