- Abstract: In the present study, the spark plasma sintering technique is used to densify pre-alloyed TiAl powders. Ti49Al47Cr2Nb2 and Ti51Al44Cr2Nb2B1 powders are sintered at temperatures ranging between 1100°C and 1250°C to yield various microstructures. Two-phased (γ+α2), duplex and lamellar microstructures are generated depending on the powder and the sintering temperature. Full compaction is achieved in a short period of time and the overall processing duration does not exceed 30min. The resultant tensile properties at room temperature are very promising whereas a limited creep resistance was obtained at 700°C [Copyright &y& Elsevier]
- Subjects :
- *SINTERING
*IRON metallurgy
*POWDER metallurgy
*TEMPERATURE
*MICROSTRUCTURE
Subjects
Details
- Language :
- English
- ISSN :
- 09669795
- Volume :
- 16
- Issue :
- 9
- Database :
- Academic Search Index
- Journal :
- Intermetallics
- Publication Type :
- Academic Journal
- Accession number :
- 34088468
- Full Text :
- https://doi.org/10.1016/j.intermet.2008.06.015