Cite
Oxidation behaviour of Mo–Si–B–(Al, Ce) ultrafine-eutectic dendrite composites in the temperature range of 500–700 °C
MLA
Das, J., et al. “Oxidation Behaviour of Mo–Si–B–(Al, Ce) Ultrafine-Eutectic Dendrite Composites in the Temperature Range of 500–700 °C.” Intermetallics, vol. 19, no. 1, Jan. 2011, pp. 1–8. EBSCOhost, https://doi.org/10.1016/j.intermet.2010.08.043.
APA
Das, J., Mitra, R., & Roy, S. K. (2011). Oxidation behaviour of Mo–Si–B–(Al, Ce) ultrafine-eutectic dendrite composites in the temperature range of 500–700 °C. Intermetallics, 19(1), 1–8. https://doi.org/10.1016/j.intermet.2010.08.043
Chicago
Das, J., R. Mitra, and S.K. Roy. 2011. “Oxidation Behaviour of Mo–Si–B–(Al, Ce) Ultrafine-Eutectic Dendrite Composites in the Temperature Range of 500–700 °C.” Intermetallics 19 (1): 1–8. doi:10.1016/j.intermet.2010.08.043.