Abstract

Abstract: Out-of-pile tritium release examinations of irradiated Li4SiO4 pebbles were performed in TRINPC-I experiments for evaluating material performance and verifying the system design. To generate tritium the specimens were irradiated with neutrons. Li4SiO4 pebbles were made by a freeze-drying method. In the experiments, concentrations of tritium in the form of tritium gas (HT+T2) and tritiated water (HTO+T2O) in the outlet streams of a reactor tube were measured separately with an ionization chamber and a liquid scintillation radiometer. The results show that the percentage of tritium gas (HT+T2) and tritiated water trapped by the breeder pebbles were about 72% and 19% of totally released tritium, respectively. Thus, more tritium was released in the form of tritium gas in this work. In addition to tritium trapped by the breeder pebbles, the amount of free tritium was also measured by breaking on-line a quartz capsule containing Li4SiO4 pebbles, the percentage of which was 9% of totally released tritium. The temperature peaks of tritium gas mainly appeared at about 477°C and 654°C, while the temperature peak of tritiated water appeared at about 402°C, under which most of tritiated water released. [Copyright &y& Elsevier]

Details

Language :
English
ISSN :
00223115
Volume :
412
Issue :
1
Database :
Academic Search Index
Journal :
Journal of Nuclear Materials
Publication Type :
Academic Journal
Accession number :
60162951
Full Text :
https://doi.org/10.1016/j.jnucmat.2011.02.018