Back to Search Start Over

Transforming growth factor-beta1 accelerates bone bonding to a blended calcium phosphate ceramic coating: a dose-response study.

Authors :
Szivek JA
Nelson ER
Hajdu SD
Yablonski K
DeYoung DW
Source :
Journal of biomedical materials research. Part A [J Biomed Mater Res A] 2004 Mar 01; Vol. 68 (3), pp. 537-43.
Publication Year :
2004

Abstract

In vivo strain measurements can facilitate the study of the bone remodeling response to loading and load changes. Calcium phosphate ceramic (CPC) coatings have been used to attach strain gauges to bone for extended periods of time, but require up to 12 weeks for adequate CPC-to-bone bonding. Transforming growth factor beta 1 (TGF-beta1), an osteoinductive growth factor, was used as a surface enhancement to accelerate bone growth and bonding to CPC particles. The aim of this study was to find an optimal dosage of TGF-beta1 to accelerate the attachment process. CPC-coated strain gauges were enhanced with doses of 0.5, 1.0, or 2.0 microg of TGF-beta1 per gauge. Gauges were placed on the femora of dogs, which were exercised daily and fed ad libitum. After 3, 6, and 12 weeks, gauge attachment was quantitatively assessed using mechanical testing and histomorphometry. Gauge attachment was also qualitatively assessed using back scatter electron microscopy. Agreement of the mechanical test results with both the back scatter electron microscopy images and histomorphometry results showed that the 1.0 microg per gauge dose of TGF-beta1 is an optimal dose to accelerate bone formation and attachment to CPC-coated strain gauges.<br /> (Copyright 2004 Wiley Periodicals, Inc.)

Details

Language :
English
ISSN :
1549-3296
Volume :
68
Issue :
3
Database :
MEDLINE
Journal :
Journal of biomedical materials research. Part A
Publication Type :
Academic Journal
Accession number :
14762934
Full Text :
https://doi.org/10.1002/jbm.a.20099