Direct surface pH determinations of setting cements.

Authors :
Charlton DG
Moore BK
Swartz ML
Source :
Operative dentistry [Oper Dent] 1991 Nov-Dec; Vol. 16 (6), pp. 231-8.
Publication Year :
1991

Abstract

Surface pH measurements were made over a 24-hour period for several luting cements and glass-ionomer lining and restorative materials. Of the luting cements, the water-mixed glass-ionomer cement, Ketac-Cem, had the lowest initial pH and the polycarboxylate, Durelon, had the highest. Three glass-ionomer lining materials showed differences in pH that increased over the entire test period. Two of the three visible-light-cured glass-ionomer liners evaluated showed similar pH values, while the third exhibited a considerably lower pH. The lower pH values found with the water-mixed glass-ionomer luting agent suggest that acidity may contribute to the posttreatment sensitivity associated with this material.

Details

Language :
English
ISSN :
0361-7734
Volume :
16
Issue :
6
Database :
MEDLINE
Journal :
Operative dentistry
Publication Type :
Academic Journal
Accession number :
1816545