Effect of Li Content, Deposition Time and Solution Concentration on Morphology and Photoluminescence Properties of Y2O3: 5%Eu3+, x%Li+ Thin Film.

Authors :
Yongqiang, Li
Lingyun, Zhang
Zhenxiang, Dai
Ganhong, Zheng
Yanan, Zhu
Yongqing, Ma
Source :
Rare Metal Materials & Engineering; Jun2017, Vol. 46 Issue 6, p1524-1529, 6p
Publication Year :
2017

Abstract

Y 2 O 3 : 5%Eu 3+ , x %Li + phosphor thin film was fabricated via an electro-deposited method. The dependence of the morphology and luminescent properties for Y 2 O 3 : 5%Eu 3+ , x %Li + thin film on Li content, deposition time and solution concentration were studied. The results indicate that the morphology and the emission intensity strongly depend on the Li content, deposition time, and solution concentration. It is found that the Li addition is beneficial to the formation of flower morphology and then enhances the photoluminescence intensity. The optimal Li content is 15% for Y 2 O 3 : 5%Eu 3+ , x %Li + . [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
1002185X
Volume :
46
Issue :
6
Database :
Supplemental Index
Journal :
Rare Metal Materials & Engineering
Publication Type :
Academic Journal
Accession number :
125253753
Full Text :
https://doi.org/10.1016/S1875-5372(17)30158-3