The Taguchi method has been used to determine the optimum conditions for the dissolution of malachite ore in H2SO4solutions. The chosen experimental parameters and their range were (i) reaction temperature: 15 to 45 °C, (ii) solid‐to‐liquid ratio: 1/10 to 1/3 g cm–3, (iii) acid concentration (in weight): 2 % to 10 %, (iv) particle size: –40 to –3.5 mesh, (v) stirring speed: 240 to 720 rpm, and (vi) reaction time: 5 to 45 minutes. The optimum conditions were found to be reaction temperature: 40 °C, solid‐to‐liquid ratio: 1/3 g cm–3, acid concentration (in weight): 10 %, particle size: –30 mesh, stirring speed: 480 rpm, and reaction time: 45 minutes. Under these optimum working conditions, the dissolution of copper and iron in malachite ore was 100 % and 58 %, respectively. Besides, alternative working conditions reducing the total cost and dissolution of iron were found.

Details

Language :
English
ISSN :
09307516 and 15214125
Volume :
24
Issue :
4
Database :
Supplemental Index
Journal :
Chemical Engineering & Technology
Publication Type :
Periodical
Accession number :
ejs2215873
Full Text :
https://doi.org/10.1002/1521-4125(200104)24:4<409::AID-CEAT409>3.0.CO;2-0