Cite
Mitigation of Erosion Wear Produced by Fly-Ash Slurry on 900 Elbow by Changing the Cross-Section Shape and Area Ratio
MLA
Ananya, Latchupatula, and Vivek Kumar Patel. “Mitigation of Erosion Wear Produced by Fly-Ash Slurry on 900 Elbow by Changing the Cross-Section Shape and Area Ratio.” Diffusion and Defect Data Part B: Solid State Phenomena, vol. 357, no. 1, June 2024, pp. 93–100. EBSCOhost, https://doi.org/10.4028/p-WP81hQ.
APA
Ananya, L., & Patel, V. K. (2024). Mitigation of Erosion Wear Produced by Fly-Ash Slurry on 900 Elbow by Changing the Cross-Section Shape and Area Ratio. Diffusion and Defect Data Part B: Solid State Phenomena, 357(1), 93–100. https://doi.org/10.4028/p-WP81hQ
Chicago
Ananya, Latchupatula, and Vivek Kumar Patel. 2024. “Mitigation of Erosion Wear Produced by Fly-Ash Slurry on 900 Elbow by Changing the Cross-Section Shape and Area Ratio.” Diffusion and Defect Data Part B: Solid State Phenomena 357 (1): 93–100. doi:10.4028/p-WP81hQ.