EVOLUTION OF OXIDE SCALES ON FeAl GRADE 3 INTERMETALLIC ALLOY

Authors :
Pedraza, Fernando
Grosseau-Poussard, Jean-Luc
Dinhut, J.F
Laboratoire d'Etude des Matériaux en Milieux Agressifs (LEMMA)
Université de La Rochelle (ULR)
Source :
Intermetallics / CHOI INTERMETALLICS, Intermetallics / CHOI INTERMETALLICS, 2005, 13, pp.27-33. ⟨10.1016/j.intermet.2004.04.042⟩
Publication Year :
2005
Publisher :
HAL CCSD, 2005.

Abstract

International audience; The ODS FeAl Grade 3 intermetallic alloy have been shown to develop a structured oxide scale upon isothermal oxidation between 850 and 950º C for 24 h. Transmission electron microscopy studies have revealed a top nanoequiaxed alumina, central alumina and bottom Fe-Al spinel. At 1000º C, the spinel phase no longer forms but a columnar alumina layer topped up with a nanoequiaxed structure. The role of yttria is negligible at lower temperatures whereas some segregation at the scale/substrate interface and precipitation of YAlO3 is observed at 1000º C.

Details

Language :
English
Database :
OpenAIRE
Journal :
Intermetallics / CHOI INTERMETALLICS, Intermetallics / CHOI INTERMETALLICS, 2005, 13, pp.27-33. ⟨10.1016/j.intermet.2004.04.042⟩
Accession number :
edsair.dedup.wf.001..daa00a1e2fac9003fe05a12d558f0420
Full Text :
https://doi.org/10.1016/j.intermet.2004.04.042⟩