Abstract
- The Pechinni method (A) as well as hydrothermal treatment (B) of co-precipitated CeO2-based gels with NaOH solution were used to synthesise pure CeO2, and CeO2-based solid solutions with formula Ce1−xMxO2, Ce1−x(M0.5Ca0.5)xO2 M = Gd, Sm for 0.15