Cite
Delamination initiation life and growth behaviour of ceramic coated steels quenched after coating process under rolling contact loading condition
MLA
Keiji Ogawa, et al. “Delamination Initiation Life and Growth Behaviour of Ceramic Coated Steels Quenched after Coating Process under Rolling Contact Loading Condition.” Materials Research Innovations, vol. 18, Aug. 2014, pp. S5-57. EBSCOhost, https://doi.org/10.1179/1432891714z.000000000910.
APA
Keiji Ogawa, Tohru Takamatsu, Hirotaka Tanabe, Motoyuki Nishizawa, & Yui Izumi. (2014). Delamination initiation life and growth behaviour of ceramic coated steels quenched after coating process under rolling contact loading condition. Materials Research Innovations, 18, S5-57. https://doi.org/10.1179/1432891714z.000000000910
Chicago
Keiji Ogawa, Tohru Takamatsu, Hirotaka Tanabe, Motoyuki Nishizawa, and Yui Izumi. 2014. “Delamination Initiation Life and Growth Behaviour of Ceramic Coated Steels Quenched after Coating Process under Rolling Contact Loading Condition.” Materials Research Innovations 18 (August): S5-57. doi:10.1179/1432891714z.000000000910.