Subcritical crack growth in multilayer Low Temperature Co-fired Ceramics designed with surface compressive stresses
- Source :
- Journal of the European Ceramic Society. 36:4095-4105
- Publication Year :
- 2016
- Publisher :
- Elsevier BV, 2016.
-
Abstract
- The strength of Low Temperature Co-fired Ceramics (LTCC) can be affected by the environmental conditions under which the material is loaded. In this work, the strength degradation associated with Subcritical Crack Growth (SCCG) mechanisms is investigated in several multilayer LTCC architectures designed with surface compressive residual stresses. The magnitude of the residual stresses was tailored combining two different LTCC materials. Biaxial strength measurements using the ball-on-three-balls method performed at room temperature in water (as reference environment) showed a clear increase in the characteristic strength with the compressive residual stress in the surface layer. The strength distribution in dependence of the surface stresses in the outer layer can be represented by a three-parameter Weibull distribution, thus providing a “threshold strength” (i.e. minimum strength) for the material. In addition, the use of compressive stresses in LTCCs introduces a threshold intensity factor for the SCCG behaviour, below which no environmental assisted cracking can occur.
- Subjects :
- 010302 applied physics
Work (thermodynamics)
Materials science
02 engineering and technology
021001 nanoscience & nanotechnology
01 natural sciences
Cracking
Compressive strength
Residual stress
visual_art
0103 physical sciences
Materials Chemistry
Ceramics and Composites
visual_art.visual_art_medium
Ceramic
Surface layer
Composite material
0210 nano-technology
Layer (electronics)
Weibull distribution
Subjects
Details
- ISSN :
- 09552219
- Volume :
- 36
- Database :
- OpenAIRE
- Journal :
- Journal of the European Ceramic Society
- Accession number :
- edsair.doi...........4eed55786649d275cb3851191316f148
- Full Text :
- https://doi.org/10.1016/j.jeurceramsoc.2016.07.003