Antireflective thin film coated by Teflon TM AF 2400 amorphous fluoropolymer to improve the pumping efficiency of disk amplifier used for laser fusion is presented. Improvement of pumping efficiency of about 8% can be attained by Teflon TM AF 2400 coating to the outer surface of Xe flashlamps and the shield glasses set up between Xe flashlamps and disk glasses. Flashlamp irradiation test to the Teflon thin film coated on flashlamp wall was carried out. Flashlamp-induced damage for 100 irradiations at about 15.4 J/cm 2 was not observed.

Details

ISSN :
0277786X
Database :
OpenAIRE
Journal :
Laser-Induced Damage in Optical Materials: 1993
Accession number :
edsair.doi...........76288441429e44ca2ef2f0cd94ba5d84
Full Text :
https://doi.org/10.1117/12.180915