Coking by metal dusting of nickel-base alloys

Authors :
Silke Strauß
R. Krajak
H. J. Grabke
Source :
Materials and Corrosion. 50:622-627
Publication Year :
1999
Publisher :
Wiley, 1999.

Abstract

Metal dusting of nickel and Ni-base alloys occurs by inward and internal growth of graphite in the metal phase, leading to extrusion and ejection of metal particles, which catalyze carbon deposition, i.e. coking. Compared to metal dusting of iron and steels which occurs via intermediate carbide formation and leads to much finer metal particles, coking on the Ni-base alloys is much less. This is caused by the larger size and smaller amount of metal particles formed by metal dusting and also by the clearly smaller rates of metal wastage on Ni-base alloys. Coking durch Metal Dusting von Nickelbasislegierungen Das metal dusting von Nickel und Ni-Basislegierungen erfolgt durch Einwartswachstum und innere Bildung von Graphit in der Metallphase, dies fuhrt zum Herausdrucken von Metallpartikeln, die dann die Kohlenstoffabscheidung, d.h. das coking, katalysieren. Im Vergleich zum metal dusting auf Eisen und Stahlen, das uber die Bildung von Karbid als Zwischenprodukt ablauft und zu sehr viel feineren Metallpartikeln fuhrt, ist das Ausmas des coking auf Ni-Basislegierungen sehr viel geringer. Dies ist bedingt durch die Grose der Partikel und ihre kleinere Anzahl und auch durch die deutlich geringeren Abtragsgeschwindigkeiten durch metal dusting bei Ni-Basislegierungen.

Details

ISSN :
15214176 and 09475117
Volume :
50
Database :
OpenAIRE
Journal :
Materials and Corrosion
Accession number :
edsair.doi...........76bebd7cdeaf480664c37c8f29c949c5
Full Text :
https://doi.org/10.1002/(sici)1521-4176(199911)50:11<622::aid-maco622>3.0.co;2-r