Electroless copper plating method combined with spark plasma sintering (SPS) was used to fabricate W-Cu alloy with low W-W contiguity. Results show that W-Cu alloy with low W-W contiguity and high relative density can be obtained by this method. With sintering temperature increased from 860°C to 1060°C, the relative density of W-Cu alloy shows a rapidly increasing tendency, but the W-W contiguity keeps at a low level. Compression testing results show that the ductility of prepared W-Cu alloy is sensitive to strain rate, and the failure strain of the W-Cu alloy shows obviously increasing tendency with the loading strain rate increased from 10-3 to 103.

Details

ISSN :
16627482
Volume :
782
Database :
OpenAIRE
Journal :
Applied Mechanics and Materials
Accession number :
edsair.doi...........a22946b452e85db8bbd6f18f0dcdf86c