The high-pressure and high-temperature synthesis of HgBa2CaCu2O6+ deltaand HgBa2Ca2Cu3O8+ deltasuperconductors and their characterization
- Source :
- Superconductor Science and Technology. 8:48-52
- Publication Year :
- 1995
- Publisher :
- IOP Publishing, 1995.
-
Abstract
- The superconductors HgBa2CaCu2O6+ delta (Hg-1212) and HgBa2Ca2Cu3O8+ delta (Hg-1223) have been synthesized by solid state reaction, carried out at 850 degrees C under 25 kbar, using the nominal composition of HgBa2Ca2Cu3Ox. The results indicate that the optimum sintering time for the Hg-1223 phase is about 0.5 h. With increasing sintering time, the Hg-1223 phase decomposes, and the Hg-1212 phase increases gradually. When the sintering time increased to 3.8 h, we obtained a sample with nearly a single phase of Hg-1212. We synthesized the HgBa2CaCu2O6+ delta superconductor under 27 kbar at various sintering temperatures using the nominal composition of HgBa2CaCu2Ox. The results indicate that the optimum sintering temperature for the Hg-1212 phase is 820-830 degrees C. The effect of annealing at various temperatures in flowing O2 on the superconductivity of HgBa2Ca2Cu3O8+ delta has been investigated.
- Subjects :
- Superconductivity
Delta
Materials science
High-temperature superconductivity
Annealing (metallurgy)
Metals and Alloys
Analytical chemistry
Sintering
Condensed Matter Physics
law.invention
Electrical resistivity and conductivity
law
X-ray crystallography
Materials Chemistry
Ceramics and Composites
Electrical and Electronic Engineering
Electroceramics
Subjects
Details
- ISSN :
- 13616668 and 09532048
- Volume :
- 8
- Database :
- OpenAIRE
- Journal :
- Superconductor Science and Technology
- Accession number :
- edsair.doi...........be63a1e146dac97a60dcd70be9ab6889
- Full Text :
- https://doi.org/10.1088/0953-2048/8/1/008