- Silicon carbide ceramics were pressureless joined by using Ti foil and Si powder, which generated Ti3SiC2 phase as the interlayer. The phase composition, microstructure and the shear strength were investigated. It was revealed that the SiC assembly after joining at 1500oC showed the high shear strength of 76.2 ± 19.5 MPa. The secondary phase of TiC within the interlayer was expected to contribute to densification improvement of Ti3SiC2 phase and thermal stress reduction.
- Subjects :
- 010302 applied physics
Materials science
Secondary phase
Process Chemistry and Technology
02 engineering and technology
021001 nanoscience & nanotechnology
Microstructure
01 natural sciences
Surfaces, Coatings and Films
Electronic, Optical and Magnetic Materials
chemistry.chemical_compound
chemistry
Phase composition
visual_art
Phase (matter)
0103 physical sciences
Materials Chemistry
Ceramics and Composites
Silicon carbide
Shear strength
visual_art.visual_art_medium
Ceramic
Composite material
0210 nano-technology
FOIL method
Subjects
Details
- ISSN :
- 02728842
- Volume :
- 46
- Database :
- OpenAIRE
- Journal :
- Ceramics International
- Accession number :
- edsair.doi...........ffbd9265c481e940976476fd98c4d01d
- Full Text :
- https://doi.org/10.1016/j.ceramint.2020.02.155