Back to Search
Start Over
Determination of high-temperature and low-humidity treatment time for larch boxed-heart timber
- Source :
- Journal of Wood Science, Vol 66, Iss 1, Pp 1-4 (2020)
- Publication Year :
- 2020
- Publisher :
- SpringerOpen, 2020.
-
Abstract
- Abstract The larch boxed-heart timbers with a cross section of 100 × 100 mm were dried after steamed at 100 °C dry-bulb temperature and 0 °C wet-bulb depression for 5 h, and then dried at 120 °C dry-bulb temperature and 30 °C wet-bulb depression for 8, 12 and 16 h, respectively, in order to determine optimal treatment time for the timber. This study indicated that the pretreatment of 12 and 16 h prevented both the surface and internal check of the timber. However, the pretreatment delayed drying time by at least 19%.
Details
- Language :
- English
- ISSN :
- 14350211 and 16114663
- Volume :
- 66
- Issue :
- 1
- Database :
- Directory of Open Access Journals
- Journal :
- Journal of Wood Science
- Publication Type :
- Academic Journal
- Accession number :
- edsdoj.3e38306a1c34d96b88c48f3167c198e
- Document Type :
- article
- Full Text :
- https://doi.org/10.1186/s10086-020-01867-2